Hi,
Here is the CAD drawing of the tray, size is 68 x 38 x 7 inches.

Here are two pictures of the wooden mould. The mould is 10mm oversized as I was aiming for 5+mm thickness, maybe thats overkill, not sure. I am just sealing it at the moment, also expecting a UPS delivery today from easycomposites.