By fx3861 - 3/25/2012 11:53:37 PM
How do I mix it? with the epoxy or hardener and for how long as the mixture usually turn cloudy aft mixing it with epoxy. Is it suppose to be that way
|
By Matt (Staff) - 3/31/2012 9:42:03 AM
Yes, that's right. It would no longer be clear when cured. Any additive (including fumed silica) will reduce the clarity of the resin when cured, particularly glass bubbles which make the resin go a white-ish colour.
|
|