Hi,
so I'm planning to make this part in CF. Plan was, coat it in a clear coat to get a smooth surface. Wax and use PVA release agent, then apply epoxy, and lay few layers of CF. (3 of 2/2 twill 400g)
Then extract the new part, and cut and do some gentle sanding with fine grit. Then, once its reasonably clean, apply a few layers of clear coat and sand those back as I hear sanding on laminating resin can go through easy.