By KingsleyHill - 5/9/2014 11:47:44 PM
I am making a new glare shield (dashboard) for an airplane. My first pass at this using a mold and carbon fiber and kevlar (strong so you can grab hold of it to get in/out of the seat) resulted in a very shiny product that while being very pretty (carbon fiber look through clear gel coat) reflected the sun and sky onto the windshield. What I need to do is make the surface as non-reflective as possible while still preserving the beauty of the carbon fiber material. How can I do that?
|
By FLD - 5/10/2014 6:51:30 PM
Well, I'm a bit pikey so I'd start with the rough side of a washing up sponge.
|
|