Talk Composites - The Forum for Advanced Composites

Ooops - measured by volume not weight, is it ruined

http://www.talkcomposites.com/Topic11206.aspx

By scrangelina - 5/9/2014 2:02:00 PM

Can anybody advise? I've mixed Addition Cure Silicone Rubber and catalyst by volume and not by weight. Might it still cure? 



By Warren (Staff) - 5/13/2014 9:25:59 AM

you should be ok on such a small error due to the similarity in density.