Talk Composites - The Forum for Advanced Composites

how to change steering wheel shape?

http://www.talkcomposites.com/Topic10970.aspx

By TomDesign - 4/28/2014 6:57:15 AM

anyone has any ideas? as i saw many companies do that. what they use any clue? as we tryed form like guys do bumpers then layed frp and sanded and carbon on top but after sun heated for and steering started to change shape. any ideas what can be used?
By TomDesign - 4/28/2014 7:51:39 AM

as like you can see Robson design they offering that. look at their facebook. and color of parts after polish like grey?any thoughts what kind of resin. as polyster gives like blue shadow, epoxy clear, vinylyster like grey.

as i wonder what can be used to change steering wheel shape as normal form is bad as from temperature always moves that why i made even bodykit from molds as after couple weeks it starts from temperatures goes like mountains in landscape.