By kylle - 1/18/2012 8:18:59 PM

I'm making a very specifc mud guard for a bike, the piece is very small, I keep following the instrutions from your videos but small air bobbles keep appearing.

The mud guard: about 10cmX6cm

http://www.talkcomposites.com/Uploads/Images/30e07a1d-6e14-4745-95aa-90a2.jpg

If you can give soma assistance! Smile
By mhdghoul - 3/18/2012 3:35:49 AM

yup ,it will be great