surface finish Help !

http://www.talkcomposites.com/Topic10852.aspx

By gambler99 - 4/18/2014 11:09:59 AM

Hello ,i'm Newbie

i have an one question.
From this video :
http://www.youtube.com/watch?v=VodfQcrXpxc

After demolding, i saw surface of carbon fiber is glossy.

but when i demolding, i get my parts surface is matt. (photo in attach files)

How to do for get glossy surface similar in video ? 
By Hanaldo - 4/18/2014 1:47:03 PM

Part is gonna be the same standard as your mould... What is your mould finished to?

Release agent has an effect too, some release agents leave a matte finish on the part.