ChrisR (17/04/2014)
oh, forgot to ask, how do you double "A" side with GC50 without having matching moulds?
Sorry missed that earlier must have been typing reply.
The only thing I have made that is similar to what your doing are Long Boards. For that I used upper and lower deck moulds and then bonded the two halves together post infusion. Spray tacked pieces of peel ply into the mould for areas needing grip before laying down the GC50. Doing it that way you can alter the core depending on rider weight, riding style and the amount of flex required whilst keeping the upper and lower skins standard.
Warren