By BambooBikeBuilder - 3/18/2012 9:29:07 PM				
            
                      
            I am building a bamboo bike frame and plan to make the joints out of carbon fibre. Some people recommend hemp as a joint because it has a similar thermal expansion coefficient. I however like the aesthetic and structural properties of carbon fibre. That being said, I have never used carbon fibre and am wondering what resin I should use. I am also debating whether to use fabric or tow. I plan to purchase the carbon fibre skinning starting kit to try it out. I will be abutting the bamboo to each other and then wrapping the carbon fibre around the joint. Are there any suggestions or books that anyone can recommend? I am very appreciative of your advice.
 
  | 			
		 
	
		
				      		    
		
		
            
            
            By DuPreez - 11/7/2013 3:52:11 PM				
            
                      
            Like the trike, definitely different. I put together a rough old design using good old paint.
           
		 | 			
		 
	
	
						
		 	
		
	 |