By thomsen - 3/25/2014 1:15:53 PM
Hi,
Aramid rapidly degraded by uv light (not only the color; strengh and stiffness decreases too).
Has "black Twaron" the same limitations?
Thomsen
|
By Warren (Staff) - 3/31/2014 12:36:23 PM
Twaron is a brand name for a Aramid fibre, so like other aramid fibres is (without additional protection or additives) succeptable to UV degredation wether dyed black or yellow in colour.
|
|