By FLD
-
3/18/2014 9:44:04 AM
Please bear in mind that I'm tight and dont like to spend money!
All my current moulds are polyester / CSM. I double gel and then lay up quite a thick mould. It polishes nicely and I've had no problems with deformation or pulling. I am very meticulous with mould release! My usual process is vac bagging but I'm thinking of going infusion. I'm not expecting large numbers of pulls from the mould. Is it worth paying the premium for unimould or should I continue with might tight-ass yorkshire approach?
By dbcrx
-
3/18/2014 7:32:09 PM
You've heard the saying "If it ain't broke, don't fix it"?
But then, I'm a tight ass too and also do most things the cheapest way possible.