By _pepis - 3/14/2014 9:45:36 AM

Hello everybody,

I got very helpful answers from you guys last time, so I decided to ask again Wink

In my infusion process I use low viscosity infusion resin. When I try to degas it with my home-made chamber I get many bubbles escaping from my pot and forming a big foam on the surface. This is endless Wink
I use full power of my vacuum pump (nearly -1.0). I've never managed to get clear liquid after degassing.

What should I do to improve it and make it more effective?

Sorry for my english,

Thanks!

Peter/Poland
By fiberpro - 5/19/2014 3:43:20 PM

I heard from technicans that it is possible to self degass resin just while infusing, have you guys tried?