Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Sheet
Carbon fibre compressive strengths
http://www.talkcomposites.com/Topic10001.aspx
By Jekyll
-
3/3/2014 12:50:49 PM
Hi I'm doing my final year project testing the compressive and flexural strengths of carbon fibre composites using your
Carbon Fibre 2/2 Twill 3k 199g 1m Wide and your EL2 laminating Epoxy using the AT30 fast hardener. I wish to estimate the strength properties of the composites before testing the samples so I have something to compare to. I know that Laminating epoxy has strengths in its technical data sheets but unfortunately there is no technical data sheets for the carbon fibre.
I would really appreciate it if you could let me inform me of some of the properties of the carbon fibre especially the compressive tensile and flexural strengths of the carbon fibres.
Kind regards
Jekyll
By Shadowbird
-
5/14/2014 3:31:06 PM
Thanks,
this information is very useful. Could you also tell me how your Resins are called?
Thanks a lot.
Eric