Depends a lot on what material you are using, fabric density, mould size etc. I have successfully infused 10 layers of 663g twill weave carbon fibre before, but had issues with infusing 7 layers of 450gsm uni. So the easiest way to answer is for you to tell us exactly what you are wanting to make etc.
|