Race seat mould with undercut's - Help needed!


Author
Message
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
You'll probably find those inserts will be moulded into the seat with large spreader plates below the CF

I do a glass fibre seat which has a ver long and slight undercut around the ribs but it releases ok so wouldn't worry about that. If it were me though with that seat, it would have to be a multi part mould and then make provision for the fasteners after
nmicro
nmicro
Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)
Group: Forum Members
Posts: 15, Visits: 151
I'm struggling to get a good mould from a race seat that i have, and I'm hoping you can give me some advice and help.

This race seat is an infuse carbon part, but it has some metal insert on booth sides, to fix it to the car, making it impossible to make a "direct" mould of it.
I believe that this metal parts are glued with some epoxy glue, so it's literally impossible to remove them.

The metal plates have around 2 ~ 2,5mm thickness and the "bolt" has around 4,5 mm.
As you can see from the pictures below, this metal parts create some undercuts and i'm not sure how can i overcome them.

The "bended" effect of the seat surroundings makes is harder to solve it.


Any help will be appreciated 

Here's some photos so you see what i'm talking about.

http://www.talkcomposites.com/Uploads/Images/d864b051-ce82-451f-a63e-46d9.jpg

http://www.talkcomposites.com/Uploads/Images/c1ef4540-932c-4175-930e-3418.jpg

http://www.talkcomposites.com/Uploads/Images/127330ed-d45a-4498-bef6-3e47.jpg

http://www.talkcomposites.com/Uploads/Images/94b8ad14-c01e-4a1c-a70e-7c0b.jpg