Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Carbon Steerin wheel project.
Carbon Steerin wheel project.
Post Reply
Like
2
Prev
1
2
Jump To Page
Carbon Steerin wheel project.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Here is repair!
Reply
Like
3
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
fiberpro i mean you just have to search right resin as after 1 year search i found resin that lay up very nice no bubbles and never appear also it brush very good. i like it a lot. only remember you do with any kind or resin for best result needs heat 50-60 celsius!
Reply
Like
3
truyentl
truyentl
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 111
i would like to do the same ,
can i use carbon fiber tape with epoxy clear coat ?
pls advise,
Thanks
Reply
Like
3
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
carbon fiber tape? we not do here anything with stickers
yes can do with epoxy resin. like i say easier to work with epoxy resin but easier to finish parts with polyster resins.
Reply
Like
3
CarZoneParts
CarZoneParts
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 7,
Visits: 71
Some upgrade after long time.
Wheel is nearly done need more wet sanding but I'm happy with results.
There is one coat of 220g CF & five coat of resin.
Also resin have some imperfection but for the first time don't look that bad. As u can see on last picture carbon fibre part match leather so both are same level.
Under light u can see resin have lotz air bubbles
any advice what i did wrong here ???
Going to do same steering wheel only will have flat bottom in carbon fibre & top with color ring on 12
Attachments
10380693_10152197179043137_9100756020468318289_o (1).jpg
(
342 views,
277.00 KB
)
Edited
11 Years Ago by
CarZoneParts
Reply
Like
2
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
how you ended carbon? i mean where join leather?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search