Hi there,

I've made a mould to produce Carbon fibre loops, the dimensions of the grooves are 5x5mm, which is the intended cross section dimensions of loops.
Initially I had an idea of taking carbon fibre loops out of mould and vacuum bagging them then i realised the might change the square cross section of loops which i want to keep.

So I wonder if vacuum bagging to whole mould with fibres in grooves will be efficient in this case or grooves too small?

And do you recommend any special arrangement of vacuum bagging materials?

Regards

Mohamed
Reply
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
noble350 (06/07/2013)
Hi there,

I've made a mould to produce Carbon fibre loops, the dimensions of the grooves are 5x5mm, which is the intended cross section dimensions of loops.
Initially I had an idea of taking carbon fibre loops out of mould and vacuum bagging them then i realised the might change the square cross section of loops which i want to keep.

So I wonder if vacuum bagging to whole mould with fibres in grooves will be efficient in this case or grooves too small?

And do you recommend any special arrangement of vacuum bagging materials?

Regards

Mohamed


Hi Mohamed
What are loops? We need a clearer description of what your are trying to do. Pictures would help.
Fred