Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Sounds like the sanding dust is showing up defects or your parts could do with a little longer to cure.
You have to be really careful with temperatures and be 100% sure where you are working IS 20C for the time other wise the cure periods will not be accurate.
Longer in the mould is better - well you cant do any harm that way. Post cure in the mould or elevated temperature cure to start with is the ideal situation.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|