Pattern Making and CAD, need advice


Author
Message
Mr Rooty Tooty
Mr Rooty Tooty
Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)Supreme Being (145 reputation)
Group: Forum Members
Posts: 15, Visits: 156
Does anyone have experience of any (cost effective) methods of taking a CAD design to tooling using commercial rapid prototyping processes?

I've been glancing at companies like Imaterialise recently and imagining the benefits of taking something directly from concept to tool Smile

When I say "cost effective" I guess what I actually mean is "If you were to use the tool to create commercial parts, would the price of commisioning the tooling be less than about 10 x the unit sale price of the components you produce from it?".

Bonobo, I've heard (and I'm no expert) that 3D laser scanners can be a nightmare to use, and the plots often require a lot of cleaning up. That said, I'd prefer to make my own mind up on this and would love to have one to play with.

Good luck!
Dave
Dave
Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)
Group: Forum Members
Posts: 48, Visits: 253
I thought you just wanted it to put your ideas onto the screen. If you want to properly design a part and then use that design to create drawings that you could make a really accurate male plug from then you really need to get hold of a proper CAD program like AutoCAD or Solidworks, I don't know much about free alternatives but these programs won't be cheap at all.

Anyway if you do get hold of a good program and you have designed your part dimensionally accurately. Create a modified version that would be perfect for a male plug aka flanges and voids filled ect. Once that is done then a good way for turning it into foam is to split your design into 25 or 50mm sections using a Section View on the program then print all the sections off. Then get corresponding thickness foam 25 or 50mm and cut them to the section prints off (Cutting slightly larger than the print offs by a few mm) and then stick your foam together and finish sanding down.
Bonobo
Bonobo
Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
I use adobe illustrator for work by the way, not sure if that would be any help for when i get into a 3D design program?
Bonobo
Bonobo
Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
Thanks! i will try one of the free ones first, i do have access to Autocad 2011, pretty hard to learn from what i've heard.
the next step will be to transfer my design to a plug, i have access to a laser cutter so i was thinking of cutting out profile sections in mdf then fill with pattern making foam block, any other methods anyone can suggest?
MJCT
MJCT
Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)Supreme Being (208 reputation)
Group: Forum Members
Posts: 18, Visits: 177
You can try Autodesk 123D Beta. SketchUp is too basic in my opinion.
Dave
Dave
Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)Supreme Being (678 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Hi Bonobo,

As your asking this question I am going to assume you don't have access to any professional CAD software. I will also assume your doing this for personal use. Aka I'll lay it out simply

Proper CAD software is not cheap so off the top of my head if you want to get your ideas out of your head and into something you want to see with no cost:  

download a free CAD program like google sketch up (other people who have more experience with free cad software maybe able to suggest something better). Then have a quick look into how to import models into sketch up and you will find there is a free public archive full of user submitted models. From this I'm sure you could find a model of an mx5 that you could import and then draw your design idea onto the car. 

This is a very basic and free way to do it. You can learn how to use sketch up very quickly as it is effectively a click and draw type of cad program where as a proper cad program will cost you and arm and a leg and several weeks of messing about to get it to do what you want although it does make turning it into a real thing a lot easier.

Dave.
Bonobo
Bonobo
Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)Supreme Being (933 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
So i'm looking at developing a ducktail style spoiler for the mx5 mk3,

i have excatly what it should look like in my head, and there's the problem! how do i get from this idea to something phisical?

firstly i will need to get accurate dimensions and shape of the boot lid from the car, the finished product needs to fit snuggly to the compound curves of the panel.

i'm sure some sort of 3d laser scanner exists, scan the car, import into autocad or similar and go from there, but this is out of reach for most of us.

I guess the another option would be to take a mould from the actual car itself then use this to make a plug?