Hi guys,

I am currently in the process of creating some patterns using your High Density Polyurethane Foam. I am planning to take them to a high gloss finish that is reasonably rugged and will withstand several moulds being duplicated off it.

I will take them to a paint shop to have to 2k primer filler applied and get it to a gloss finish as i don't have good enough equipment for 2k paint. Is it possible for the paint shop to get the finish i want just using 2k filler primer?

Secondly how should i prepare the foam for them? Should i coat it in a thin layer of FG tissue and resin or will it be fine bringing it to them showing foam?

I'm just look to sort out any issues before i look around for a good body shop to do the work. As i will need it done relatively quickly once the foam is done.



Thanks,
Dave.
Reply
Dave
Dave
Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)Supreme Being (662 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Hi will, i hadn't noticed there was another reply on this topic! I am based in cardiff.

Thanks,
Dave.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search