Hey guys. Interested in improving upon my carbon layup technique with small radius, small overall sized parts.

Here's my most recent bike -> http://dillerdesign.com/random/bike/fat_bamboo_v2/DSC_0185.JPG

...and my first one (yikes, what I know now...) -> http://dillerdesign.com/random/bike/bamboo_01.jpg

I'm doing experiments of late involving inflation membranes (vs a full inflation bladder) and any alternative to vacuum bagging, as my parts don't have any flat reference plane to tape to / is generally a big pain in the butt =)

Hoping to be building custom carbon and bamboo frames commercially in 2013!
Replies
prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Cool bikes.

What type of material have you used for your bladders?

Drew Diller (14/03/2013)
[quote]fgayford (14/03/2013)

I've been playing with making my own bladders, and I definitely see the appeal.



http://motoform.blogspot.se

Drew Diller
Drew Diller
Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)Supreme Being (248 reputation)
Group: Forum Members
Posts: 35, Visits: 199
prsw (14/03/2013)
Cool bikes.

What type of material have you used for your bladders?

I didn't intend to, and I still have to work out a show stopper problem when going higher than 30 psi, but to answer your question:

Smooth-On's reusable vac bag silicone. I originally bought a test batch to do just that, vacuum bagging. It can stretch more than 200% in practice and remain in one piece. I used word "playing" seriously, as I don't have it working to what I'd call effectively yet. At any rate, I can see the potential.

I originally got interested in the stuff after experiencing some bridging in my most recent frame, of which I do not have any decent pictures out of embarrassment. I overheated a bamboo pole through too might infrared light. I also put the bottom bracket shell in backwards... ugh. I hunt it up in my garage as a monument to what happens when I get impatient.
prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
ok, thanks.
This method seems interesting but I think I will start with tubular bag folded back on itself,
or latex bicycle inner tub.


http://motoform.blogspot.se

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Drew Diller - 12 Years Ago
matthieutje65 - 12 Years Ago
Drew Diller - 12 Years Ago
fgayford - 12 Years Ago
Drew Diller - 12 Years Ago
fgayford - 12 Years Ago
prsw - 12 Years Ago
Drew Diller - 12 Years Ago
prsw - 12 Years Ago
Drew Diller - 12 Years Ago
Drew Diller - 12 Years Ago