Hi, i want to increase the thickness of some aluminium sheet by adding several layers of carbon fibre to the one side of it. However I want the finished piece to have structural strength not just cosmetic.
My plan was to produce the carbon panels first with several layers of reinforcement using a vacuum bag and peel ply on one face, then fix to the aluminium panels via a structural glue rather then epoxy resin.

Thoughts would be welcome ,thanks 