Hi, I have the structure below which, under solicitations, is bending a bit towards the direction of the red arrows.
Pipes are 40mm diameter.
I was thinking about moulding two half pipes composed mostly of several layers of unidirectional carbon tape and then glue with mma the half pipe to the existing pipes (along the orange lines).
The layup I am thinking is 10x layers of 50mm wide 650gm2 carbon unidirectional tape, alternated with some 50mm wide plain carbon tape.

What do you think about the idea and the layup schedule?

Also, maybe adding a 2 mm pvc core in between would help? I am just worried that the shear force could cause the two carbon frames to slip on the pvc core, so maybe a not cored layup would be better?


Replies
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
If you add plates to the marked plane on both sides of the structure, and bolt them every few inches the stiffness should improve quite much. if you only find shorter plates you might just cover the middle area around the thinnest section.

Attachments
20210219_150803.jpg (143 views, 86.00 KB)
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
oekmont - 2/19/2021 2:15:07 PM
If you add plates to the marked plane on both sides of the structure, and bolt them every few inches the stiffness should improve quite much. if you only find shorter plates you might just cover the middle area around the thinnest section.

Thank you!!!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 4 Years Ago
SleepingAwake - 4 Years Ago
Hanaldo - 4 Years Ago
mporta71 - 4 Years Ago
Hanaldo - 4 Years Ago
mporta71 - 4 Years Ago
oekmont - 4 Years Ago
             This could be doable too, thank you
mporta71 - 4 Years Ago
mporta71 - 4 Years Ago
SleepingAwake - 4 Years Ago
mporta71 - 4 Years Ago
oekmont - 4 Years Ago
Hanaldo - 4 Years Ago
oekmont - 4 Years Ago
             Thank you!!!
mporta71 - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search