Hi everyone, in the quest of making a carbon fiber timing belt cover for the engine of my car i understood i need to use the high temperature resin and cure the part to "unlock" its properties.
Since it's my first project i'd like to keep expenses low to not waste money in case i give up and i tried to see if i could come up with something.
I would like to know if a curing oven set up like this would work:
-600x600 wooden box, with all 6 sides made of 3mm osb wood panel, 50mm insulation panel and again 3mm osb wood panel on the outside
- Temperature regulator ITC-2000 (up to 100°C) (https://www.amazon.it/Inkbird-Temperatura-Riscaldamento-Raffreddamento-Calibrazione/dp/B0185M6I28/ref=sr_1_1?__mk_it_IT=%C3%85M%C3%85%C5%BD%C3%95%C3%91&dchild=1&keywords=itc-2000&qid=1602081498&sr=8-1)
- 2000W Heating element (https://www.amazon.it/Victool-Ceramic-Ceramica-Elemento-riscaldante/dp/B08GQP692W/ref=sr_1_1_sspa?__mk_it_IT=%C3%85M%C3%85%C5%BD%C3%95%C3%91&dchild=1&keywords=elemento+riscaldante+1000w&qid=1602080802&sr=8-1-spons&psc=1&spLa=ZW5jcnlwdGVkUXVhbGlmaWVyPUExWU83MlUxTEc3TUhBJmVuY3J5cHRlZElkPUEwNDQxNDY1MU5UU01RRUFKNUdRSCZlbmNyeXB0ZWRBZElkPUEwNDY1MDcwMkE5T05JMkg4T1I4TiZ3aWRnZXROYW1lPXNwX2F0ZiZhY3Rpb249Y2xpY2tSZWRpcmVjdCZkb05vdExvZ0NsaWNrPXRydWU=
- 220v  circulating fan (https://www.amazon.it/VENTOLA-120x120x38mm-220-230V-CUSCINETTI-METALLICO/dp/B00PZWAA2G/ref=sr_1_7?__mk_it_IT=%C3%85M%C3%85%C5%BD%C3%95%C3%91&dchild=1&keywords=ventola+220v&qid=1602179544&sr=8-7)

I would make a small partition in the box to house the heating element, with some holes to circulate air in the main partition with the fan

It's around 50€ for the electronics, with the materials for the wooden box and wiring i think i should spend around 100€ while in other topics i've read of people spending 4 times as much.
The question is, would this work to cure a small part at the requested 60° for 6 hours? is the wood going to be a fire hazard with this setup?
Edited 5 Years Ago by AleHachiRoku
Reply
Dentex
D
Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)Supreme Being (404 reputation)
Group: Forum Members
Posts: 42, Visits: 1.4K
I am also searching about DIY ovens so I guess I can help. 

My idea is also to build wooden frame with "box in a box" like design with insulation around. But I think that 3mm mdf might be too thin, someone will correct me if I am wrong.
I envisioned it like this: build wooden frame, cover it outside with 10mm MDF, cover inner sides with rock or fiberglass wool (100mm) and make another box with top from steel sheet of 0.5-1mm thickness that will be attached to frame also. Door would open from top, like a chest. I hope you get the idea.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
AleHachiRoku - 5 Years Ago
Hanaldo - 5 Years Ago
Rosta Spicl - 5 Years Ago
AleHachiRoku - 5 Years Ago
Rosta Spicl - 5 Years Ago
Dentex - 5 Years Ago
Hanaldo - 5 Years Ago
AleHachiRoku - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search