Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Should be totally fine. At 60C, the element is barely going to be on, so there isn't much risk. My MDF oven has been going strong for 4 or 5 years now, and I use it virtually every day as high as 150. I would probably be a little more comfortable using MDF rather than OSB, but at 60 I really don't think it will be an issue.
I'm also not totally sold on that fan. I would look for an OEM oven fan - these have the fan on a shaft so that the motor stays outside the oven. Also dirt cheap, so worth considering. Again, probably more of a concern for going to higher temperatures, but just my 2c.
|