Group: Forum Members
Posts: 2,
Visits: 25
|
Hi,
I have no experience with Carbon fibre and do not understand anything about it so need someone to rest my mind.
I have just bought a second hand bike and the carbon fibre frame looks distorted at parts (I’ve attached two videos).
Does this mean the carbon fibre isn’t genuine or is this just a poorly made frame?
Could it cause any problems in the long term?
Cheers, Lewis
|