Epoxy over chrome


Author
Message
carbon man
carbon man
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hi, can I use high temperature epoxy tooling get coat straight over chrome to mould off? 
oekmont
oekmont
Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
If "straight over" involves a release agent then yes.

carbon man
carbon man
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
oekmont - 7/4/2020 9:56:49 AM
If "straight over" involves a release agent then yes.

6 coats of easy lease? 

oekmont
oekmont
Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Should work if done properly.