	Group: Administrators 	        
    Posts: 214, 
    Visits: 782 
    
 
          
		     | 
				                       
                 
                
                    
			            dont trust the temperature read out on the oven.  Buy yourself a thermometer to check it. 
  If your curing something in a vacuum bag eg resin infused etc then you have no worry about fumes as its all sealed.
  If you are postcuring parts or not using a bag then you will want to run the oven afterwards with the door ajar at 100 degrees for 20 minutes just in case you have any fumes.  Same really if you bake lacquered parts off in the oven.  Running it low temp with oven door ajar means the fan blows out any slight build up of solvents.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |