			            Hi, 
 I have a question regarding the use of Easy-Lease. I did a mould from a carbon fiber part using EG60 Gelcoat and the corresponding EG60 paste. As a release agent I used Easy-Lease. I applied 6-8 layers of Easy-Lease, and there was more than 1 h after the last layer. Then 2 layers of gelcoat, and finally the paste...
 
 But then, impossible to release the part. It actually was completely stuck to the Gelcoat. I manage to get the part back using screw driver, hammer, sand paper...
 
 I am trying to figure out why that is. I have used Easy-Lease in the past...no problem. The only thing I can see is that I have my Easy-Lease stock for more than 1 year, and it has in fact been open more than a year ago. I know its shelf-life is 1 year from production...I have ordered a new stock...but I am trying to figure out if just getting out of date would be a sufficient reason for this problem...just that I keep a better track of the dates of my release agent in the future. Or should this not be such an issue  and I should look elsewhere to explain this problem ? But then, I really have no clue what could go wrong...
 
 Thanks!
 
 
 |