Group: Forum Members
Posts: 550,
Visits: 27K
|
The picture is very bad. As you found the crack, I guess you can see it from the outside. What do you mean by "internal"? Is it an endoscope picture? If so, the crack seems to go from the outside inwards, through the whole laminate.
Sorry for your friend, but you can say that a crack like this only happens through an external forces. Additionally, carbon composites have excellent alternating load propertys. If the frame made 2 years without getting this crack, it is extremely unlikely that it will get damaged by regular use.
I am pretty sure that something happens to this frame. Maybe an impact, maybe jamming or inappropriate clamping during transportation.
|