Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Be wary of any rattle can high build primers or primers. They are heavily solvent based and would need a proper oven cure to stop them degassing during the mould making process. What happens is the release agent then fails where the paint is and the mould will stick in those areas. Bodyfiller does the same too in many cases.
Properly sprayed 2k paints fully oven cured are normally ok though.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|