Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
perforated bleeder ply
perforated bleeder ply
Post Reply
Like
6
perforated bleeder ply
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
MarkMK
MarkMK
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 338,
Visits: 2K
EC sell this product, plus 'Bread Wrap' film which has some similar applications
https://www.easycomposites.co.uk/200g-red-22-twill-3k-carbon-fibre-cloth
It's used as a release film where bleeding of the resin through the film is also required. It is commonly used between the fabric and the breather layer in vacuum bagging and allows the breather layer to be released easily from the part once cured. The breather layer aids the evacuation of air from the part and acts to soak up excess resin when vacuum is applied
It can also be used during infusion, typically when using a woven infusion mesh that doesn't tear quite so easily and helps to remove it from the cured part
Edited
7 Years Ago by
MarkMK
Reply
Like
4
ian.kelly@basegroup.co.uk
ian.kelly@basegroup.co.uk
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 21
I've seen some how to videos that show the use of a perforated bleeder film in the vac bag stack but I'm having trouble tracking it down. Why is it used? Is breather fabric the same thing? Is there a film that I can use and punch my own holes.
this is one of the videos
https://youtu.be/T4ZFj4fItWE
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search