	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            Without degassing, it can be difficult to get the air out the brick underside. You will have to pour it in stages. Sometimes poking with a cocktail stick helps.  Pouring the resin just over the brick, then gently wafting with a heat gun can be enough to make it sink into the brick voids.                
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |