			            Hey everybody,
  I want to build a front wing depending on the original part with Prepreg. For sure it has to be a two part mould. My problem is how to get the two parts bonded because the edge line will be only about 1mm and so it is too small to make a bonding. I have some ideas and hope to get some input:
  1. after making the two parts I go for a smaller version. I make a second carbon part using the first carbon Part as „mould“. This way I get a smaller part which can be used as connecting part to bond the two main parts together. 
  2. I lay up the two moulds with a little overlap on one part, put them together, insert a bladder and make a small hole on the downside to inflate the bladder. But actually I have never tried this technique. I get it in theory but I do not now what to use as bladder and how much pressure is necessary. 
  3. same as number two but using a silicone plug which should expand with heat and produce enough pressure for the Prepreg. In this case I would be happy to get some tips about how to make the silicone plug, especially where to get the right material. 
  4. last idea: filling each mould with polystyrene foam and use the foam to produce pressure. But I do not know if the foam will produce enough pressure and how to fix the flaps. 
  So you See, lots of questions :] perhaps some of you understand what I try to do and give me some input. 