Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
Issue with hand layup carbon part
Issue with hand layup carbon part
Post Reply
Like
7
Issue with hand layup carbon part
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Damien
Damien
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 32,
Visits: 132
Hello,
I have an issue with my hand layout carbon fiber parts...
It looks like the resin does not fill in the carbon part really well...see photo
Here is my process:
- Mold with gel coat and easylease release agent (I have no problem releasing the part)
- Temperature 23-25 C
- This part (but I get the same with all parts) is 1 carbon (1st layer) and 3 glass
- I use a 1.3:1 in weight for the amount of epoxy vs material
- I use the easycomposite roller to remove air bubbles etc...at each layer. This time, even, to try and see if it would help, I used a heat gun on each layer to get rid of micro-bubbles. But made no difference.
- Then I put a release tissue, a perforated film and a layer of
special
foam to absorb the excess of epoxy.
- Vacuum bagging overnight
But still I get this...which gives me lots of work to give it a proper finish afterwards...
Any idea what I do wrong ?
Thanks !
Attachments
20190526_104715_resized.jpg
(
661 views,
867.00 KB
)
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Issue with hand layup carbon part
Damien
-
7 Years Ago
Pretty standard for wet lay vac bagging, it isn't as easy to get a good surface finish as it is with infusion. Probably pulling too much vacuum and squeezing too much resin out, leaving a resin...
Hanaldo
-
7 Years Ago
Oh ! Too much vacuum is something I did not consider ! Thanks for the tip ! I will reduce it and try. Thing is that infusion seems a bit tricky for a newbie like me !
Damien
-
7 Years Ago
Nah the thing with infusion is that as long as you follow the process correctly and don't cut corners or rush, it will guarantee your part comes out perfectly (provided your mould is perfect of...
Hanaldo
-
7 Years Ago
For wet bagging your resin should equal the amount of cloth. If your cloth weighs 1000 grams then you should mix an equal amount of epoxy. Too much resin will cause the excess resin to shrink...
JasonFL
-
7 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search