Unfortunately you will struggle to get those deep bubbles out. You could try drilling or grinding a hole down to them then re-filling it, but chances are it may still show up once cured. Bubbles near the surface are easier to deal with. Also the fresher the resin pour, the less likely you will see the repair as there fresher the pour the more cross-linking will occur.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|