Group: Forum Members
Posts: 155,
Visits: 992
|
I talked to the supplier about the distorted surface. They agreed most likely voids between laminate and coat that pushed out dimples when air heated. They recommended bagging the mold after wet lay to pull out air. I assume this is also going to pull out all excess resin so I probably need to go plenty of layers to get a good thickness. If I do it this way, can I pretty much ignore any air during wet lay and let the vac bag handle it? Resin has an hour pot life but I would still like to move pretty fast to get plenty of layers and get it bagged. Is all air gonna work it's way out?
|