The edges can be machined or finished by hand to get a smooth edge. The uniform black finish is probably painted with a matt black paint. Typically you would see a charcoal black colour on the edge with some very slight lines showing the layers. Alternatively some people brush a thin layer of resin or cyanoacrylate glue over the edge to seal and protect, or you can just polish/wax it with a wax rich black coloured polish.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|