The oil separator filter is not designed to be user washable so you would have to be very careful if you were to try and rinse it out.  We can order in spares for the pump if you have a clogged filter.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
JasonFL
JasonFL
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 51, Visits: 707
Geteda - 10/18/2018 12:47:29 PM
This resin cure fast, manufacturer say 6hr, but im demoulding at 24hr, same results.

EDIT: Tested on flat mold of polyester gelcoat, its OK, thanks.


Did the chemical release fix your problem?

Jason
Geteda
Geteda
Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)Supreme Being (103 reputation)
Group: Forum Members
Posts: 15, Visits: 58
JasonFL - 4/9/2019 10:23:27 PM

Did the chemical release fix your problem?

Hi
Yes, I have solved the problem with the release agent, now I am using frekote 700-nc.
Would be great to be able to buy the Easy-Lease Chemical Release Agent but it is impossible, it can not be imported.