Hi. I want to cast a rod of approx 12mm diameter that I can heat and bend once cured. What would be a good choice of resin for this? I have some alumilite dyes that I'd like to use so ideally it would be compatible with these. Thanks, Tom


Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
bellacboy - 10/15/2018 7:08:56 PM
Hi. I want to cast a rod of approx 12mm diameter that I can heat and bend once cured. What would be a good choice of resin for this? I have some alumilite dyes that I'd like to use so ideally it would be compatible with these. Thanks, Tom


Castable resins are thermoset and cannot be bent with heat.