Top coat of resin tacky


Author
Message
C4RBON94
C
Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)Supreme Being (136 reputation)
Group: Forum Members
Posts: 9, Visits: 25
Hi I've just nearly finished my first carbon fibre skinned parts and the final coat has had over 50 hours to dry yet is still tacky, guessing this points to an incorrect ratio of hardener to resin?? What's the best way to fix this as I have tried to compiucoit which removes the tackiness but leaves a meatt finish

Tia , apologies if this is in the wrong place
GO