Will be in big trouble if I photograph these !!!! For example From the centre of 1 fork end to the other is say 150mm When you print your fork at the ends in the exact centre of each you print your 6mm hole You have a plate with 2 6mm studs pr bolts protruding with the centres at 150mm Push the 2 studs into your printed holes Your part is held at the right centre during cure Once at room temp remove plate/studs
|