Questions about the use of Xencast PX30


Author
Message
Asurada
Asurada
Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)
Group: Forum Members
Posts: 10, Visits: 954
I'm trying to use PX30 to make a flexible mold, this resin is very flexible, but his tear resistance is poor, I bend it with my hand, it can bend a lot of angle, but when I twist it, it will easily break and crack.
Is this because of the properties of the resin? I can confirm that my blending ratio is no problem, why does it have such a problem? Or there are no other rubber-like resins, I would like to take to make a flexible resin mold, for casting silicone hand ring.I'm trying to use PX30 to make a flexible mold, this resin is very flexible, but his tear resistance is poor, I bend it with my hand, it can bend a lot of angle, but when I twist it, it will easily break and crack. Is this because of the properties of the resin? I can confirm that my blending ratio is no problem, why does it have such a problem? Or there are no other rubber-like resins, I would like to take to make a flexible resin mold, for casting silicone hand ring.I'm trying to use PX30 to make a flexible mold, this resin is very flexible, but his tear resistance is poor, I bend it with my hand, it can bend a lot of angle, but when I twist it, it will easily break and crack. Is this because of the properties of the resin? I can confirm that my blending ratio is no problem, why does it have such a problem? Or there are no other rubber-like resins, I would like to take to make a flexible resin mold, for casting silicone hand ring.



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search