I'm looking for some general advice on making an intake plenum to suit a low boost turbo engine (7 PSI) out of carbon fiber using vacuum infusion, utilising my 3D printer to create the mould. This would be the first carbon fibre part that I've made, based on a design drawn up in Autodesk Fusion 360 shown below.

So far I've spent a few days doing research online, reading other posts in this forum relating to intake manifolds and 3D printing moulds and watched numerous videos on producing carbon fibre parts. However I still have a few open points I'd like to get peoples opinion on. 
  • Based on the plenum shape I'm assuming I would create a positive mould.
  • Should I use tooling gel or something like 3M Super 77 sparingly to ensure the CF attaches to the shape.  
  • Does this sound right to create a 3D printed mould; use PLA filament, smooth down the edges, spray a few coats of plastic filler primer and seal with S120 mould sealer.
  • For the 4 bolt end flange I'm guessing this can't really be formed using CF. Instead could I go about inserting an aluminium flange that could form part of the mould and be covered in CF. Would this hold up under boost? 
  • Layer up wall thickness to be around 2mm, from what I've read this would be strong enough.
I'm happy to post pics as I go a long, I'm currently doing prototype prints of the mould. 

Reply
Steve Broad
Steve Broad
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
An old post but, just in case the OP is still here.

I would reconsider making the plenum out of carbon. A friend, who builds race cars, stopped me from doing just this.

On a N/A engine there shouldn't be any issues. However, a turbo engine is a different matter. The pulsing that occurs in the plenum is such that there is a risk of the carbon failing and being sucked into the engine, which happened to my friend.

The small saving in weight isn't worth risking an engine.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
bytesandbolts - 7 Years Ago
oekmont - 7 Years Ago
bytesandbolts - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search