			            On curved pieces you can still get a great effect, however you need to be a bit more patient as you can only build up thin layers so you will need to apply several thin layers of resin (much like carbon skinning) then once the build up is thick enough, allow it to fully cure and then you can wet sand it and polish to get a nice smooth high gloss finish like you would on a flatter piece of wood. 
 
 Warren Penalver
 Easy Composites / Carbon Mods - Technical Support Assistant
 
 |