Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Realistically a 2 piece mould otherwise you will struggle to demould it with vertical edges. Once you have a mould, you could wet lay, infuse or pre-preg. All 3 would work.
Which option depends on equipment available, experience and the size and hence practicality of one method over the other.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|