Suitable epoxy resin to seal a 3D printed mould
Suitable epoxy resin to seal a 3D printed mould
Post Reply
Like
5
Suitable epoxy resin to seal a 3D printed mould
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
joei.pavlas
j
joei.pavlas
posted 8 Years Ago
ANSWER
HOT
Topic Details
j
Group: Forum Members
Posts: 5,
Visits: 72
Hi,
I make some parts using carbon prepreg (from Hexcel) and 3D printed Polycarbonate moulds. To make a glossy surface finish of the moulds, I use 2-3 layers of
XTC 3D
(more closely unspecified epoxy resin) with sanding between each layer. Finally I seal the surfaces with S120 Mould Sealer from Easy Composites (10 coatings). Resulting carbon part looks amazing, but I have a problem with the mould. The XTC 3D does not stick to Polycarbonate very well, so after demoulding there are small areas on the mould sourface, where the layers of XTC 3D are peeled off. Because of that, I can't use the mould again without any repair of the surface. Interesting is, that the resin from carbon prepreg stick very well to the Polycarbonat. On places, where is not release agent applied, I'm not able to peel off the resin from the surface.
Can someone recommend me some type of epoxy resin or gelcoat as a replacement of the XTC 3D? It can be also a resin from Easy Composites portfolio. I also require applicability of the resin up to 100°C and fast curing time (preferably up to 2hrs at elevated temperature - 60-80°C )
Thanks in advance!
Tags
Board Sealer
S120
Edited
8 Years Ago by
Warren (Staff)
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Suitable epoxy resin to seal a 3D printed mould
joei.pavlas
-
8 Years Ago
HelloI did a similar mold for trial.It was 3D printed out of Polymaker PC-PlusThe cavities were sanded, then I used easylease as release agent. Once prepreg was cured, I had difficulties to pop the....
Tony2125
-
8 Years Ago
The issue is the temperature requirement. 100C pushes you into the high temperature system realms. Eg our EL160 High Temp Epoxy Laminating Resin which will go to 160C with an appropriate oven post....
Warren (Staff)
-
8 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search