Resin compatability with paint


Author
Message
Junior
Junior
Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Decided to go for 1k lacquer and it looks great but it just hasn't got the durability I desired and is scratching too easily Sad

I now have the dilemma of what to do next. I have been advised a 2k lacquer won't go over a 1k lacquer which means i'd have to strip it back down and re-paint.

Would the XCR resin go over the 1k lacquer if keyed first?

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The trouble with going over a 1k lacquer is that 1k lacquers never properly harden. So you go over the top of it with a nice hard 2k or epoxy or whatever, but the 1k coating underneath still moves around and shrinks and outgasses etc, and it effects the 2k coating over the top of it. So if you are after durability you are much better off removing the 1k coating and restarting.
Junior
Junior
Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)Supreme Being (830 reputation)
Group: Forum Members
Posts: 73, Visits: 473
I thought epoxy had a certain degree of flex to it? How come it doesn't crack on materials such as wood that expand and contract?
oekmont
oekmont
Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)Supreme Being (8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Wood is a solid Material, 1k laquer isn't. The epoxy might glue to the very surface, but in the end, everything ontop of the 1k laquer just floats on the painted object.
1k rattle can laquer is really not a good idea for basically anything that needs mechanical surface protection.