Hi,
recently I made a piece in prepreg under vaccum in an oven over the night (8h) and in the morning there were a lot of oil evaporation (like a fog) in the room and the oil level of the pomp was very low and around the pomp  was oil as it as was coming out of the chimney. Also the pomp made a louder noise then usually.
But I did check the oil level before using the pomp. 
Could you tell me where this problem is coming from?
Thanks in advance
Christophe
Saff
Saff
Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)
Group: Forum Members
Posts: 10, Visits: 723
Adelbolide - 10/8/2017 8:49:14 PM
Hi,
recently I made a piece in prepreg under vaccum in an oven over the night (8h) and in the morning there were a lot of oil evaporation (like a fog) in the room and the oil level of the pomp was very low and around the pomp  was oil as it as was coming out of the chimney. Also the pomp made a louder noise then usually.
But I did check the oil level before using the pomp. 
Could you tell me where this problem is coming from?
Thanks in advance
Christophe

usually vacuum pump produce oil fog when it is pumping air, when a good vacuum level is reached the fog produced is minimal. perhaps your vacuum bag was non perfectly sealed?


my facebook page
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Adelbolide - 10/8/2017 8:49:14 PM
Hi,
recently I made a piece in prepreg under vaccum in an oven over the night (8h) and in the morning there were a lot of oil evaporation (like a fog) in the room and the oil level of the pomp was very low and around the pomp  was oil as it as was coming out of the chimney. Also the pomp made a louder noise then usually.
But I did check the oil level before using the pomp. 
Could you tell me where this problem is coming from?
Thanks in advance
Christophe

Hi Adelbolide,

Saff is exactly right - the VP435 vacuum pump (in common with most rotary vane vacuum pumps) will produce oil vapour when the pump is extracting air; if the bag is properly sealed then once all the air is extracted then the amount of oil vapour produced should be negligible (almost zero). Therefore, one of two things has happened;

1) The bag was not properly sealed in the first place (i.e. it always had a small leak) and therefore the pump has effectively been pulling air out of the bag all night.
2) The bag (or seal) punctured whilst in the oven. This most often happens if the bag is pulled tight near a taped seam - when the tape gets hot in the oven it softens slight and can move - if the bag is stretched tight near a seam like this then it can break the seal. Another way a previously properly sealed bag can puncture when it's put in the oven is during loading - sometimes the act of placing the part into the oven can puncture the bag, particularly if you have a metal shelf and a full 'envelope' vacuum bag surrounding the mould.

For this reason, we don't recommend running the pump unattended just in case a leak develops within the bag during the cure. *At the very least*, you would certainly want to be present whilst the part comes up to temperature and for as much of the cure as possible.

I hope this helps,

Best regards, Matt


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search